1 The J. M. Ney Company, Bloomfield, Connecticut 06002
A method of casting tensile rods, and a simplified method of fusing porcelain disks to the rods for measuring bond strength in a repeatable manner, are described. Bond strengths as high as 20,000 psi were recorded on oxidized rods. Both chemical depletion and a coating of gold reduced the bond.
Submitted on May 1, 1968